| Material | Max Temp | Density | Corrosion | Best For |
|---|---|---|---|---|
| PP Polypropylene | 100°C | 0.91 g/cm³ | Good — most acids, alkalis, salt solutions | Acid scrubbers, water treatment, general low-temperature corrosive service |
| PVDF Polyvinylidene fluoride | 150°C | 1.78 g/cm³ | Excellent — strong acids, chlorides, halogens | Chlorine/HCl service, higher-temperature acid scrubbers, high purity |
| PTFE Polytetrafluoroethylene | 260°C | 2.2 g/cm³ | Outstanding — virtually inert | Most aggressive media, hot concentrated acids, high purity |
| SS304 Stainless Steel 304 | ~400°C (mechanical) | 7.93 g/cm³ | Good — clean atmospheric and mild chemical | Clean hydrocarbons, general distillation, non-chloride service |
| SS316 / 316L Stainless Steel 316 / 316L | ~400°C (mechanical) | 8.0 g/cm³ | Very good — molybdenum resists chlorides and acid gas | CO₂/H₂S service, amine units, marine, sour gas |
| Duplex Duplex / Super-duplex stainless | ~300°C | 7.8 g/cm³ | Excellent — high chloride and stress-corrosion resistance | High-chloride service, seawater, high stress |
| Ceramic Chemical porcelain / alumina ceramic | >1000°C | 2.3–3.9 g/cm³ | Outstanding — acids and high temperature | Hot acid manufacture, high-temperature gas scrubbing |
| Carbon Carbon / graphite packing | High (non-oxidising) | ~1.5 g/cm³ | Excellent — HF, strong oxidising acids | HF service, strong oxidisers that attack ceramic and metal |
What to Avoid
- PP: Strong oxidisers, aromatic hydrocarbons, hot chlorine, >100°C
- PVDF: Strong hot alkalis, some polar solvents
- PTFE: Molten alkali metals, fluorine gas (limited)
- SS304: Chlorides, wet H₂S, hot acids
- SS316 / 316L: Strong reducing acids, hot concentrated chlorides
- Duplex: Strong reducing environments
- Ceramic: HF and fluoride media, thermal shock, mechanical impact
- Carbon: Strong oxidising atmospheres at high temperature